0
RESEARCH PAPERS

Relation Between Wear of Cr.Ni Steels and Debris Transport at High Temperature (950°C)

[+] Author and Article Information
D. Play, M. Godet

Laboratoire de Mécanique des Contacts, Institut National des Sciences Appliquèes de Lyon, 69621 Villeurbanne Cedex, France

J. of Lubrication Tech 102(2), 247-251 (Apr 01, 1980) (5 pages) doi:10.1115/1.3251488 History: Received June 18, 1979; Online November 17, 2009

Abstract

Visualization of the friction process of a Cr.Ni Steel pin running on a disk of similar material under nitrogen has shown that a built-up edge (b.u.e.) is gradually formed and eliminated at contact. The construction of the b.u.e. is described. Metallurgical sections of b.u.e. formed under different conditions are analysed and confirm mechanisms suggested by visualization. Both visualization and b.u.e. examinaton point to the importance of flow transport in friction processes.

Copyright © 1980 by ASME
Your Session has timed out. Please sign back in to continue.

References

Figures

Tables

Errata

Discussions

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related Journal Articles
Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In